Controlled Crystallisation Of Ti02 In Alkali-Borosilicate Glass And Its Bactericidal Properties

The influence of thermal processing on Ti02 crystallisation in alkali-borosilicate glass was investigated applying differential thermal analysis, X-ray diffraction analysis and electron microscopy. The surfaces of the samples prepared by both volume and surface Ti02 crystallisation were evaluated from the viewpoint of their respective bactericidal properties.