Control Of Stresses During Production Of Sheet Glass

A study has been made of the processes by which stresses are initiated and redistributed in a glass ribbon during the forming of flat glass and in sheets of glass. This was based on a mathematical simulation of the relevant processes derived from numerical solution of boundary values of the mechanics of a deformable solid and heat conduction using finite element analysis. Measurements on laboratory specimens and under production conditions were also made. The results have been used for microprocessor control of new-generation flat glass lehrs developed by the Steklomash organisation.

Author
S E Umanskii, B I Pokrass
Origin
Unknown
Journal Title
Glass And Ceramics 1989 46 5-6 245-249
Sector
Special Glass
Class
S 5023

Request article (free for British Glass members)

Control Of Stresses During Production Of Sheet Glass
Glass And Ceramics 1989 46 5-6 245-249
S 5023
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.