Contribution To Spectrographic Analysis Of Si02-Bearing Materials For Glass Manufacture. (In German)

The spectographic determination of Fe2O3, Al2O3, TiO2, MgO, Ca0, Ni0, Co203, Cr203, V205, Mo03 and Zr02 in silica materials for glass manufacturer in discussed, including variations using amorphous carbon (total combustion) and graphite (partial combustion) as the electrode materials.