Contribution To The Size Effect On The Strength Of Flat Glass

The ASHRAE diagram for the required thickness of rectangular glass plates with simply supported edges under uniform load is analysed and the maximum principal tensile stresses are calculated for two selected load levels.

Author
K Blank, H Gruters, K Hackl
Origin
Rheinisch-Westfalische Technische Hochschule, Aachen
Journal Title
Glastech Ber 1990 63 5 135-140
Sector
Flat glass
Class
F 217