Contitioning Offered Major Improvements

As machine speeds get faster in the glass container industry and tonnages increase, it is becoming more difficult to condition the glass effectively. FIC (UK) has been working on this problem in conjunction with Glass Service and a series of solutions have been modelled demonstrating the potential for major improvements.