Continuous Measurement Of The Dissolution Rate Of Ions From Glasses

A method for measuring the early stage ion release of gases was developed in order to gain information on leaching kinetics and chemical resistance of glasses in aqueous environments. A continuous flow-through-reacotr was designed in which the aqueous solution is fed through a bed of glass particles and the dissolved ions continuously recorded with a sensitive on-line analysis system. Experimental parameters, such as solvent flow rate and temperature, could easily be adjusted according to the needs. The flow-through-reactor system was tested with powdered samples of float and lead glasses, E-glass and bioactive glasses 45S5 and 1-98, all of which showed very different chemical durability in aqueous environments.

Author
S. Taipale Et Al
Origin
Abo Akademi Univeristy, Finland
Journal Title
Advanced Materials Research Vols 39-40 (2008) 341-346
Sector
General
Class
G 3519a

Request article (free for British Glass members)

Continuous Measurement Of The Dissolution Rate Of Ions From Glasses
Advanced Materials Research Vols 39-40 (2008) 341-346
G 3519a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.