Continuous Flow Dilution Equation As A Tool In Judging And Controlling Changes In Glass From A Continuous Glassmelting Furnace

The simple exponential equation first proposed by W.M Hampton accurately represented the data for rate of change in a continuous glassmelting furnace. A tabulation, useful in a simplifying calculations, is presented. A procedure is outlined for making accelerated colour changes, and data from an actual change are presented. A relation between transit time (time for batch introduced at the doghouse to become part of the glass at the forming position) and homogeneity is suggested. The differential form of the exponential equation change from observation of the rate of change as represented by density measurements.

Author
A.K. Lyle.
Origin
Unknown
Journal Title
American Ceramic Society Bulletin 1969 48 (12) 1118-1121
Sector
Primary Papers
Class
PP 643

Request article (free for British Glass members)

Continuous Flow Dilution Equation As A Tool In Judging And Controlling Changes In Glass From A Continuous Glassmelting Furnace
American Ceramic Society Bulletin 1969 48 (12) 1118-1121
PP 643
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.