Continuous Control Of Glass Viscosity At The Forehearth Exit - Conditioning Control Based On Constant Viscosity Rather Than Constant Temperature

The availability of an on-line viscosimeter with a precision comparable to current temperature measurements allows a shift from temperature controlled glass conditioning to a viscosity controlled glass conditioning. In such a way, all variations of viscosity including non-thermal viscosity changes are monitored and can be taken into account by new process control strategies such as predictive system and the use of fuzzy control system.

Author
H Hessenkemper
Origin
Tu Bergakademie Freiberg, Germany
Journal Title
Int Glass Journal No 92 April-June 1997 54-56
Sector
General
Class
G 1618

Request article (free for British Glass members)

Continuous Control Of Glass Viscosity At The Forehearth Exit - Conditioning Control Based On Constant Viscosity Rather Than Constant Temperature
Int Glass Journal No 92 April-June 1997 54-56
G 1618
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.