Container Makers Cooperate In Gaseous Emissions Research

Portugal's glass technology institute CTCV has been measuring the atmospheric outputs of container plants. A revision of the best available techniques in the glass manufacturing industry is being prepared. The article provides a resume of principal gaseous emissions of the Portuguese container glass sector and looks at various abatement technologies currently in use, considering the impact of IPPC legislation in more detail.

Author
Un-named
Origin
Unknown
Journal Title
Glass July 2006 11