Container Glass Expansion In Russia And Ukraine

It has been reported that Sisecam has agreed a loan of over 64M Euros from the EBRD to finance the expansion of its subsidiary, Andolu Cam, in the Russian and Ukrainian glass beverage container sectors. The expansion will include the construction of an additional furnace with a 330/tpd capacity and the cold repair and expansion of the existing furnace at Kirishi (Russia), as well as the construction of a furnace at a brownfield plant in Odessa, Ukraine, with a capacity of 230/tpd. The project will enable Sisecam's Odessa plant to grow and compete with Western Imports.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide March-April 2009 9
Sector
Container glass
Class
C 3902

Request article (free for British Glass members)

Container Glass Expansion In Russia And Ukraine
Glass Worldwide March-April 2009 9
C 3902
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.