Container Coating - Improved Quantity And Reduced Costs

The relative advantages of different hot and cold end coating chemicals are discussed. The recent development of postcoating compositions for filling lines is also described.

Author
J Von Samson
Origin
Th Goldschmidt Ag
Journal Title
Glass January 1990 19-21
Sector
Container glass
Class
C 271