Considerations And Results In Applying Oxygen Firing To Industrial Glass Melters

Glass manufacturers constantly confront the challenge of maintaining a cost-effective operation in the face of tightening environmental regulations. Converting glass melters to 100% oxy-fuel firing is becoming a popular alternative to deal with this problem and minimize future restrictions placed on their operation. This paper reviews the results from several recent oxy-fuel melter conversions and field trials.