Concentrations And Site Partitioning Of Fe2+ And Fe3+ Ions In A Soda-Lime-Silica Glass Obtained By Optical Absorbance Spectroscopy

Iron-doped glasses with nominal mol% consumption 15Na2O-15CaO-70SiO2, melted under oxidising and reducing conditions, and in most cases refined with sodium sulphate, have been analysed by optical absorbence spectroscopy over a wide range (3000-35000cm-1). The Fe2O concentration was varied from 0.05 to 2 mol% and some of the glasses were co-doped with CeO2, reduced with carbon, or oxidised with NaNO3. The developed mathematical fitting analysis revealed that Fe2+ and Fe3+ ions both occupy octahedral and tetrahedral sites. Both types of Fe2+ sites were found to be Jahn-Teller distorted, i.e. elongated, by fitting the transmission absorbence spectra.

Author
T T Volotinen Et Al
Origin
Sheffield University, Uk
Journal Title
Phys Chem Glasses 49 5 2008 258-270
Sector
Special Glass
Class
S 3507

Request article (free for British Glass members)

Concentrations And Site Partitioning Of Fe2+ And Fe3+ Ions In A Soda-Lime-Silica Glass Obtained By Optical Absorbance Spectroscopy
Phys Chem Glasses 49 5 2008 258-270
S 3507
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.