Concentration Changes Of Potassium In Glasses During Electron Microprobe Analysis

The way in which the intensity of the characteristic x-rays decreases with time has been investigated to find the effects of thickness of the evaporated conductive film, electron beam diameter, beam intensity and type of evaporated material. The best working conditions for quantitative microanalysis of silicate glasses can be determined.