Computer Simulation For Thermoelastic Impact On Glass

The critical radial stress generated on the flat surface of a brittle material during low-velocity thermoelastic impact can be calculated using a computational method instead of analytical methods. The computer program presented here can be utilized to calculate, as a function of time and position, the critical radial stress generated in the vicinity of a thermoelastic impact site. It was observed that this program can also be utilized to predict the surface damage pattern that would be generated on surfaces of brittle materials that are thermoelastically impacted.

Author
R Ackakaya
Origin
Sisecam Research Centre, Turkey
Journal Title
Proc Xvii Igc Beijing, 3 Glass Properties 1995 21-26
Sector
Special Glass
Class
S 1273

Request article (free for British Glass members)

Computer Simulation For Thermoelastic Impact On Glass
Proc Xvii Igc Beijing, 3 Glass Properties 1995 21-26
S 1273
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.