Computer Control Cuts Melting Costs

Experience with the Glassmaster system on a three-port cross-fired furnace capable of melting 220 tons daily from a melting area of 65 square metres is described.

Author
J P Hartley
Origin
Redfearn Plc
Journal Title
Glass Industry October 1989 14-20, 35