Computational Study Of Four-Fold Coordinate Boron In Borates: Assignment Of Dge-Shared Structures

Several issues raised by the recent discovery of compounds with four-fold coordinate boron in edge-shared pairs are addressed by means of first principles computations. First, site-specific assignments are made by computing the quadruple coupling of each boron and comparing literature values. Then, the bonding contacts in this unusual arrangement are studied through the atoms-in-molecules approach. Finally, the unusual three-fold coordinate oxygen in another high pressure borate phase is studied in the same way. All computations were performed using the projector-augmented wave formalism.

Author
J W Zwanziger
Origin
Dalhousie University, Halifax, Canada
Journal Title
Phys Chem Glasses B 53 1 2012 7-10
Sector
Special Glass
Class
S 4185

Request article (free for British Glass members)

Computational Study Of Four-Fold Coordinate Boron In Borates: Assignment Of Dge-Shared Structures
Phys Chem Glasses B 53 1 2012 7-10
S 4185
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.