Computational Modelling Of Glass Container Forming Processes

The last decade has seen research into numerical modelling of glass production processes flourish as a result of recent advances in computer power. This paper provides an overview to the background of numerical techniques used in the IFORM code for modelling the forming process on an IS machine. An example is provided to show how these models may be used to undertake sensitivity studies to investigate the effect on final wall thickness to changes in gob temperature and plunger uptimes.

Author
G Q Liu Et Al
Origin
Rockfield Software Ltd
Journal Title
Int Glass Review 2 1998 57-59
Sector
Container glass
Class
C 1273

Request article (free for British Glass members)

Computational Modelling Of Glass Container Forming Processes
Int Glass Review 2 1998 57-59
C 1273
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.