Computation Of Three-Dimensional Temperature And Convective Flow Profiles For An Electric Glass Furnace

A first attempt has been made to obtain a numerical solution of the the three-dimensional equations of energy and momentum transfer and heat generation in an electric glassmelting furnace. In view of thecomplexity of the problemthe calculations were limited to a consideration of the convective flow profiles produced by a given voltage within a 2.12 x 2.12 x 2.12 m space with rigid boundaries.

Author
C. Tai-Seng And R.E. Goodson
Origin
Unknown
Journal Title
Glass Technology 1972 13 (6) 161-167
Sector
Primary Papers
Class
PP 628

Request article (free for British Glass members)

Computation Of Three-Dimensional Temperature And Convective Flow Profiles For An Electric Glass Furnace
Glass Technology 1972 13 (6) 161-167
PP 628
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.