Computation Procedure For The Temperature In Hot Glass. Application To The Finite Element Simulation Of Hollow Glass Forming

A new incremental procedure is developed for the thermal analysis in 3D glass products considering the one-dimensional analytical solutions for a semi-infinite glass wall. When coupled to a code being capable of computing large mechanical deformations, this allows the glass flow during pressing, self-deformation and blowing processes to be analysed efficiently. The forming of a reference tumbler is analysed via finite element simulations. For each forming step, the temperature distribution is calculated from the pressing parameters; pertinent results are found for this first application.

Author
D Lochegnies Et Al
Origin
Unknown
Journal Title
Glastech Ber Glass Sci Technol 69 8 1996 253-264
Sector
Special Glass
Class
S 1060

Request article (free for British Glass members)

Computation Procedure For The Temperature In Hot Glass. Application To The Finite Element Simulation Of Hollow Glass Forming
Glastech Ber Glass Sci Technol 69 8 1996 253-264
S 1060
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.