Computation Of The Maximum Torque Of A Cap Liner Using A Power-Law Friction And Finite Element Analysis

This work looks at the experimental study and the finite element analysis of the maximum torque of a metal cap with a liner over a glass bottle. The cap liner is hyperelastic. The predicted maximum torque is then calculated by a numerical integration scheme over the contact surface, using an experimental coefficient of static friction (power-law) as a function of the normal pressure. The predicted torque shows good agreement with that measured through experiments.

Author
A Lajmi Et Al
Origin
Unknown
Journal Title
Packaging Technology & Science 22 Dec/2010
Sector
Container glass
Class
C 4299

Request article (free for British Glass members)

Computation Of The Maximum Torque Of A Cap Liner Using A Power-Law Friction And Finite Element Analysis
Packaging Technology & Science 22 Dec/2010
C 4299
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.