Compressive Strength Of Bioactive Sol-Gel Glass Foam Scaffolds

Larry Hench's 45S5 Bioglass has been used in over a million patients as a synthetic bone graft, in the form of a particulate. Bioglass is able to stimulate more bone regeneration than other bioactive ceramics. However, it is not commercially available as a porous scaffold with amorphous glass structure because the composition crystallises during sintering. The sol-gel foaming process was developed in Hench's laboratory to overcome this problem. This paper reviews the work on scaffold development from Hench's group and reports new data that shows maximum compressive strengths in excess of 5 MPa can be achieved while maintaining the interconnected pore networks required for vascularised bone ingrowth. This was achieved through optimisation of sintering of the sol-gel foams. Sintering of the sol-gel foams was correlated to the network connectivity and silanol content. Changes in strength after immersion in simulated body fluid were found to be small over the times investigated. Relating the dissolution results to in vivo studies indicates that the scaffolds degrade more rapidly in vivo than in vitro.

Author
G Poologasundarampillai Et Al
Origin
Imperial College London
Journal Title
Int J Appl Glass Sci 7 2 2016 229-237
Sector
Special Glass
Class
S 4255

Request article (free for British Glass members)

Compressive Strength Of Bioactive Sol-Gel Glass Foam Scaffolds
Int J Appl Glass Sci 7 2 2016 229-237
S 4255
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.