Compositional Dependence Of Cdse Quantum Dot Formation On Silicate Host Glass Composition

Silicate glasses were synthesized with additional CdO and ZnSe of varying content. When CdO was added up to 3 mol% with the amount of ZnSe fixed at 1 mol%, absorption due to Se2 colour centres significantly decreased and the colour of glasses as bleached without any evidence of CdSe quantum dots. However, characteristic absorption due to CdSe quantum dots appeared without additional heat treatment when the ZnSe content exceeded 1.5 mol%, whereas the CdO content was fixed at 1 mol%. Raman spectra and transmission electron microscopy verified the formation of CdSe quantum dots.

Author
Y Lee Et Al
Origin
Kongju National University, Chungnam, Korea
Journal Title
Jacs 96 12 2013 3868-3871
Sector
Special Glass
Class
S 4081

Request article (free for British Glass members)

Compositional Dependence Of Cdse Quantum Dot Formation On Silicate Host Glass Composition
Jacs 96 12 2013 3868-3871
S 4081
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.