Compositional Changes During Electron Microprobe Analysis Of Alkali Silicate Glasses.

Local changes of compositions of alkali silicate glasses with time of electron bombardment during electron micro probe analysis are observed. The concentration of an element in the probed region varies with time in different ways depending upon the glass composition, the intensity of electron beam and the composition and thickness of conducting coating. The results are summarised as follows: Generally the xray intensities of the alkali metals is more rapid for higher beam loadings. Moreover, high beam loadings cause the increase of the xray intensities of the alkali metals in the low alkali glasses.

Author
R Hayami & H Wakabayashi
Origin
Unknown
Journal Title
J Ceram Soc Japan 78 896/4 1970 138-47
Sector
Primary Papers
Class
PP 1322b

Request article (free for British Glass members)

Compositional Changes During Electron Microprobe Analysis Of Alkali Silicate Glasses.
J Ceram Soc Japan 78 896/4 1970 138-47
PP 1322b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.