Composition Of The Volatile Phase Of Fluorophosphate Crown Glasses (Russian)

Results of experiments have confirmed the losses predicted by calculation and indicate that the volatilisation products contained relatively high amounts of fluorine and phosphorous. The formation of compounds of the type POF3 and PF5 is considered probable.

Author
O.S. Volkkov Et Al
Origin
Unknown
Journal Title
Neorganischeskie Materialy 1974 10 (12) 2249-2250
Sector
Primary Papers
Class
PP 961