Composition Of Titania Coatings Deposited By Different Techniques

Quantitative element concentrations in titania films produced by different deposition techniques (evaporation, sputtering, ion-assisted deposition, ion plating and dip coating) have been determined by means of Rutherford Backscattering Spectrometry and Nuclear Reaction Analysis. Large differences of the hydrogen content are found for the various production techniques and the related deposition parameters, which correlate with the refractive index of the respective film.

Author
C Ottermann Et Al
Origin
Schott Glaswerke, Germany
Journal Title
Glastech Ber 67 4 1994 87-92
Sector
General
Class
G 1061

Request article (free for British Glass members)

Composition Of Titania Coatings Deposited By Different Techniques
Glastech Ber 67 4 1994 87-92
G 1061
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.