Composition And Working Properties Of Ancient Glasses

M suggests the application of the ceramists laboratory skills and techniques as an aid in tracing technological development of glass making. The available literature on ancient glass composition is summarised. Two tables cite range in composition of ancient and modern glass, and typical analyses of Egyptian, Roman and Babylonian glass.

Author
R Frederick And J Matson
Origin
Unknown
Journal Title
Chem.Education 28 2 1951 82-87
Sector
Primary Papers
Class
PP 1390