On The Complete Analysis Of Alkali Lime-Silicate Glasses And Raw Materials For Glass By Means Of Atomic Absorption

Various methods are described which allow silicate samples to be dissolved without losses of the components determined occurring during the solution. In addition to the components, which can be determined by routine analysis at present, it is now possible to determine higher concentrations of SiO2 and Al2O3 in the test solution. The determination of silica however involves major errors. The solution under pressure using hydrofluoric acid is described in detail.

Author
G Medicus
Origin
Unknown
Journal Title
Silikattechnik 23 10 1972 345-347
Sector
Primary Papers
Class
PP 1298

Request article (free for British Glass members)

On The Complete Analysis Of Alkali Lime-Silicate Glasses And Raw Materials For Glass By Means Of Atomic Absorption
Silikattechnik 23 10 1972 345-347
PP 1298
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.