Comparison Of The Society Of Glass Technology Method Of Analysis Of Soda Lime Glass With That Employed By The (Belgian) National Glass Institute.

An outline of the 2 methods of determining SiO2, SO3, R2O3,CaO,MgO,Na2O,K2O,MnO,As2O3,Fe2O3, and TiO2 of an N.B.S sample of dolomite is given. The 2 procedures are compared in flow-sheets. The 2 methods gave similar results for soda lime glass. (22 tables)