Comparison Of The Optical Cutoffs Of Bismuth Borate And Bismuth Germanate Glasses

Glasses containing heavy metal oxides are often candidates for linear and nonlinear optical applications but the relationship between the optical properties and structure has not been thoroughly investigated. This study reports on the optical mobility gaps and mobility gap tails of bismuth borate and bismuth germanate glasses.

Author
D Stentz Et Al
Origin
Coe College, Usa
Journal Title
Phys Chem Glasses 41 6 2000 406-408
Sector
Special Glass
Class
S 2110