Comparison Of Glass Fragments By Neutron Activation Analysis

A method of comparing glass fragments of potential application to forensic science has been developed and evaluated. A representative sample of window glass from England and Wales has been collected and analysed for about 25 elements. An automated radiochemical separation followed by gamma-spectroscopy was used in order to determine the concentration of the maximum number of elements. Frequency distributions of the elemental concentration are showna nd used to assess the discrimination of the technique and compare it with the measurement of refractive index. A few simulated cases have been included to demonstrate the possible application to forensic science problems.

Author
R F Coleman & G C Goode
Origin
Atomic Weapons Research Est, Uk
Journal Title
J Radioanalytical Chemistry 15 1 1973 367-388
Sector
Special Glass
Class
S 1269

Request article (free for British Glass members)

Comparison Of Glass Fragments By Neutron Activation Analysis
J Radioanalytical Chemistry 15 1 1973 367-388
S 1269
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.