Comparison Of Direct And Indirect Selective Laser Sintering Of Porous Apatite Mullite Glass Ceramics

The feasibility of using the layer manufacturing technique of selective laser sintering (SLS) for the fabrication of custom made bioceramic bone implants has been investigated here.