Comparative Study Of Glass Flow In Flat Glass Tank Furnaces (In Russian)

Data are presented on glass flow in two Fourcault tanks. A transfer study of the dynamics of glass flow have provided information on the sharpness of the division and the relative force of the free-flow and working flow cycles, the part played by barriers and transverse convection.