A Comparative Method Of Checking Angles On Glass Samples

An optical method of checking angles on glass samples is described. The method is comparative: the reference is a polished sample, the angle of which has been measured on a precision goniometer. It has the advantage that angles with either polished or fine ground surfaces can be measured since use is made of reflections off the faces of the angle at close to grazing incidence. Angles with fine ground surfaces can be checked to 5 seconds of arc and with polished surfaces to 2 seconds of arc.

Author
Dw Harper
Origin
Unknown
Journal Title
Journal Of Scientific Instruments 1 6 1968 687-689
Sector
Primary Papers
Class
PP 1411

Request article (free for British Glass members)

A Comparative Method Of Checking Angles On Glass Samples
Journal Of Scientific Instruments 1 6 1968 687-689
PP 1411
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.