Comparative Analysis Of Several Heat-Resistant Glasses For Tableware (In Chinese)

Glass tableware, especially heat-resistant glass, are used more and more in daily life. Because of the different materials the performance and quality of the glass varies substantially. Based on experiments, the performances of several glassware types were analysed.