Combustion Separation Techniques In Glass Analysis

The combustion method is suitable for the separation and determination of volatile components of glass: fluorine, boron, sulphur and chloride in glass as well as carbon and sulphur in sand. Comparison with other methods demonstrates the efficiency of the combustion method.