Combustion Modifications For Control Of Nox Emissions From Glass Melting Furnaces

Results of field trials on two commercial container furnaces are presented and recommendations made on design and operation to minimise nitrogen oxides emissions.

Author
H A Abbasi, D K Fleming
Origin
Unknown
Journal Title
Ceramic Engng Sci Proc 1988 9 3-4 159-167
Sector
General
Class
G 184