Colour Separators Offer Improved Sorting

The use of recycled glass in the furnace provides both environmental and financial benefits, however, with the range of different glass colours being produced, recycling plants are relying on the development of more advanced sorting methods to help process the waste glass.

Author
P Mayer
Origin
Unknown
Journal Title
Glass 78 7 August 2001 222, 224