Colloidal Processing Of Sic Whisker Composites

In this paper, the dispersion processing and the characterisation of the dispersity of SiC whiskers for reinforced ceramic-based composites were studied. Two kinds of methods were used to determine the dispersity of SiC whiskers. First, the sedimentation density was employed to directly characterise the dispersity of the SiC whiskers. The other is an indirect characterisation.