A Collaborative Study Into The Determination Of Boron In Glass Using X-Ray Fluorescence (Xrf) Spectroscopy

XRF spectrometry is extensively used for production factory control because of its high precision and rapidity of response. For very accurate boron determinations in glass, classical wet chemical methods are still the preferred method of choice as the x-ray irradiation of light elements produces only a weak fluorescent response. However, the new generation XRF instruments employing enhanced matrix correction models plus the greater availability of certified reference materials may significantly improve the analytical performance of XRF spectrometers of rate determination of"difficult" elements such as boron.

Author
E Guadagnino
Origin
Staziione, Italy
Journal Title
Glass Technology 47 4 2006 103-111
Sector
Special Glass
Class
S 3219

Request article (free for British Glass members)

A Collaborative Study Into The Determination Of Boron In Glass Using X-Ray Fluorescence (Xrf) Spectroscopy
Glass Technology 47 4 2006 103-111
S 3219
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.