Cold End Spray Coating Equipment

Thermal and coating equipment specialist Vidromecanica recently presented its new equipment for cold-end coating of glass containers by spraying above the conveyor belt. At Glassman Europe 99 in Lyon, the Portuguese company displayed the fully automatic machinery which sprays glass containers with a dilute polyethylene wax emulsion. An external coating with good slip properties is thus created on the glass container. Vidromecanica says features of the equipment include a portal frame and a bridge with traverse sliding guides for the spray gun trolley, which can also be moved lengthwise in order to compensate belt motion. These traverse and lengthwise motions are made by a DEW motor reudcer with position control and are automatically synchronized according to the belt speed. The spraying between rows is very precise.

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 4/99 64
Sector
News Items
Class
N 671

Request article (free for British Glass members)

Cold End Spray Coating Equipment
Gmpa 4/99 64
N 671
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.