Cold Chemical Welding Of Silica Furnace Crowns

Silica is and will remain the dominant refractory for the crowns of glass melting furnaces in the foreseeable future. It has a relatively low cost and a high chemical purity suitable for the conditions of glass melting. The main factors limiting the service life of the silica crowns are the maximum working temperature up to 1620 deg C, the limited resistance to alkaline corrosion and rat-holing.

Author
Prof S Lutskanov
Origin
Lubisol Eng, Bulgaria
Journal Title
Glass Technology 44 5 Oct/03 173-175
Sector
Refractories
Class
R 535

Request article (free for British Glass members)

Cold Chemical Welding Of Silica Furnace Crowns
Glass Technology 44 5 Oct/03 173-175
R 535