Coating Of Carbon Fibres - The Strength Of The Fibres

The 6k carbon fibre Torayca T800H was coated with pyrolytic carbon by a CVD process. Fibre bundles were tested and evaluated. By this procedure, the whole distribution of the failure prabability with respect to the fibre strength is obtained in a single experiment.