Coat Bottles With Micro-Thin "Glass" Barrier Layer

Airco Coating Technology have developed a process for plasma-enhanced chemical deposition of clear silica coatings on PET, polyethylene polycarbonate or other plastics bottles to provide an oxygen barrier comparable to metallised film.

Author
M H Naitove
Origin
Unknown
Journal Title
Plastics Technology 1990 36 13 39
Sector
Container glass
Class
C 390

Request article (free for British Glass members)