Coal Gasification For Melting Glass

Of all energy used by the glass industry, 85% is natural gas, which has increased in cost over the last 10 years from around $3 to $14M BTUs at the major wholesale markets. Energy prices have had a huge impact on manufacturing cost. For example, energy now represents 20-25% of the total manufacturing cost for the container industry, compared with 10% just a few years ago. If the industry is to remain in business, the cost of energy must be reduced and price stability needs to be obtained to permit reliable long-term planning. Syngas (synthetic gas) from clean coal gasification (CCG) technologies, may provide a part of the answer. This article examines the technology in more detail.

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 85 9 2006 10
Sector
General
Class
G 3228

Request article (free for British Glass members)

Coal Gasification For Melting Glass
Am Ceram Soc Bull 85 9 2006 10
G 3228
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.