Co2 Reduction From Glass Melting Furnaces By Oxy-Fuel Firing Combined With Batch/Cullet Preheating

About 30% fuel savings and 20% reduction in CO2 emissions have been demonstrated in an oxy-fuel fired container glass furnace combined with batch/cullet preheating, as compared with a state-of-the art regeneartive furnace. An advanced oxy-fuel fired glass melting furnace with a new batch/cullet preheater is projected to reduce the specific fuel consumption further to 2.65 GJ/mton and specific CO2 emissions to 237 Kg/ton.

Author
H. Kobayashi, Et Al
Origin
Praxair
Journal Title
www.Praxair.com/Praxair.Nsf/Allcontent/7Ed5857E77A3D7888525723B006Cc5A2/$File/P-9730%20-%20Co2%20Reduction%20From%20Glass%20Melting%20Furnaces%20By%20Oxy-Guel%20Firing%20Combined%20With%20Batchcullet%20Preheating.Pdf
Sector
General
Class
G 4094

Request article (free for British Glass members)

Co2 Reduction From Glass Melting Furnaces By Oxy-Fuel Firing Combined With Batch/Cullet Preheating
www.Praxair.com/Praxair.Nsf/Allcontent/7Ed5857E77A3D7888525723B006Cc5A2/$File/P-9730%20-%20Co2%20Reduction%20From%20Glass%20Melting%20Furnaces%20By%20Oxy-Guel%20Firing%20Combined%20With%20Batchcullet%20Preheating.Pdf
G 4094
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.