Classical And Differential Thermal Analysis Studies Of The Glass-Ceramic Transformation In A Ysialon Glass

Nucleation and crystallization studies were conducted on a YSiAlON glass that contained 17 equiv.% nitrogen (7.5 at.%) by using a two-stage nucleation-and-growth treatment. Classical and differential thermal analysis (DTA) techniques were both used to study the crystallization process, to ensure that the optimum heat-treatment schedule that yielded a fine microstructure and minimum residual glass was applied.

Author
R Ramesh Et Al
Origin
University Of Limerick, Ireland
Journal Title
J Am Ceram Soc 81 5 1998 1285-1297
Sector
Glass Ceramics
Class
GC 310

Request article (free for British Glass members)

Classical And Differential Thermal Analysis Studies Of The Glass-Ceramic Transformation In A Ysialon Glass
J Am Ceram Soc 81 5 1998 1285-1297
GC 310
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.