Clarification Of Cooling Water In Glass Factories: Process Set Up And Plant Sizing (In Italian)

Different clarification processes of cooling water used in secondary glass manufacutring are compared. A most effective, economic treatment consists of the addition of a flocculant to accelerate sedimentation of suspended particles, the water clarification in a sedimentation basin and filtering of the slurries. This treatment makes clean cooling water available with marked advantages for manufacturing process quality and equipment maintenance.

Author
S Vitolo Et Al
Origin
Unknown
Journal Title
Rivista Della Staz Sper Del Vetro 26 6 1996 281-289
Sector
General
Class
G 1589

Request article (free for British Glass members)

Clarification Of Cooling Water In Glass Factories: Process Set Up And Plant Sizing (In Italian)
Rivista Della Staz Sper Del Vetro 26 6 1996 281-289
G 1589
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.