Chinese Glass Fibre

The Chinese glass fibre industry has seen rapid growth in production and sales in the last 2 years, with a rise to 2.35M/t in 2008 - up from 1.6M/t in 2007 - an increase of 44.4%. This article takes a look at the Chinese glass fibre market and assesses how it has performed in the last 12 months.