Chinese Container Glass - Outcomes And Ideas From A National Forum

At the last count, production capacity for container glass in China was in the region of 20M tonnes/pa. In the first of a two part review of the Chinese container glass industry, Meng Lingyan, Chairman of the Executive Council of China Naitonal Association for Glass Industry (CNAGI), discusses his own personal views on some of the challenges facing the sector. Part two will be published in the August/September edition of Asian Glass.